Fused silica brick is also called zero-expansion silica brick or thermal shock-resistant silica brick. They have extremely low thermal expansion coefficient, excellent resistance to rapid cooling and rapid heating, and good high-temperature performance. They are widely used in the rapid repair of various coke ovens.

Parameter of fused silica brick
| アイテム | 溶融石英レンガ |
| SiO2 ( %) | ≥98 |
| アル2○3 ( %) | ≤0.3 |
| 鉄2○3( %) | ≤0.5 |
| CaO( %) | ≤0.2 |
| Bulk Density (g / cm3) | ≥1.8 |
| Apparent Porosity ( %) | ≤20 |
| Cold Crushing Strength(MPA) | 30以上 |
Advantages of fused silica bricks
- Fused silica bricks are of high purity and corrosion resistance
- The thermal expansion coefficient of fused silica bricks is small
- The thermal shock resistance of fused silica bricks is low
- Fused silica bricks have high viscosity at high temperatures, 高強度, 強い耐スラグ性, strong impact resistance, 低熱伝導率, and small shrinkage during drying and firing.